Improved Experimental Procedure for Determining the Punching Strength of Reinforced Concrete Flat Slab Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Improved Experimental Procedure for Determining the Punching Strength of Reinforced Concrete Flat Slab Structures

Author(s): A.E. Long and D.M. Masterson

Publication: Symposium Paper

Volume: 42

Issue:

Appears on pages(s): 921-938

Keywords: columns (supports); compressive strength; connections; flat concrete plates; flat concrete slabs; loading rate; models; punching shear; reinforced concrete; shear strength; stress transfer; tests

DOI: 10.14359/17315

Date: 1/1/1974

Abstract:
A series of 12 tests was performed on reinforced concrete flat slab models of 1/6 scale to determine their ultimate punching strength under combined shear and transfer of moment loading.