Title: Shear Stength of Slabs with Moments Transferred to Columns

Author(s): N.M. Hawkins

Publication: Symposium Paper

Volume: 42

Issue:

Appears on pages(s): 817-846

Keywords: building codes; columns (supports); concrete slabs; connections; flat concrete slabs; moments; reinforced concrete; shear strength; shear tests; stress transfer; torsion

DOI: 10.14359/17311

Date: 1/1/1974

Abstract:
A study is made of available data concerning the shearing strength of slab-column connections without shear reinforcement when moment transfer occurs between the slab and the column.