Title: The Behavior and Design of Reinforced Concrete Corbels

Author(s): G. Somerville

Publication: Symposium Paper

Volume: 42

Issue:

Appears on pages(s): 477-502

Keywords: corbels; detailing; failures; loads (forces); modulus of elasticity; reinforced concrete; reinforcing steels; reasearch; shear strength; structural design; tensile stress; tests

DOI: 10.14359/17298

Date: 1/1/1974

Abstract:
The behaviour of reinforced concrete corbels is examined in detail by referring to experimental data. Previous design methods evolved as a result of this data are presented and compared.