Title: Failure of Deep Beams

Author(s): R.F. Manuel

Publication: Symposium Paper

Volume: 42

Issue:

Appears on pages(s): 425-440

Keywords: beams (supports); compression; cracking (fracturing); deep beams; failure; flexural strength; reinforced concrete; shear strength; structural design

DOI: 10.14359/17295

Date: 1/1/1974

Abstract:
A method of predicting the capacity of deep beams is presented and compared with the prediction methods of other authors and with test results. The proposed method of shear capacity prediction is based on a web compression mode of failure rather than the usual diagonal tension mode of failure and appears to have some basis in existing test evidence. A design procedure is included.