Influence of Repeated Loading On the Stirrup Stress of Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Repeated Loading On the Stirrup Stress of Reinforced Concrete Beams

Author(s): J. Ruhnau

Publication: Symposium Paper

Volume: 42

Issue:

Appears on pages(s): 169-182

Keywords: beams (supports); crack width and spacing; cyclic loads; fatigue (materials); loading rate; reinforced concrete; stirrups; stress transfer; structural analysis; web reinforcement

DOI: 10.14359/17283

Date: 1/1/1974

Abstract:
Usually the stirrup stresses of test beams are measured during initial loading. The validity of this stress-load relation is discussed in regard to design criteria of web reinforcement, inclined crack width control, and fatigue strength of web reinforcement.