Performance Evaluation of a Partially Prestressed Rigid Frame Concrete Bridge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Performance Evaluation of a Partially Prestressed Rigid Frame Concrete Bridge

Author(s): Arvid Grant and John H. Clark

Publication: Symposium Paper

Volume: 23

Issue:

Appears on pages(s): 625-630

Keywords: bridges (structures); continuity (structural); deflection; girders; live loads; partial prestressing; performance tests; post-tensioning; precast concrete; prestressed concrete; reinforced concrete; rigid frames; structural design

DOI: 10.14359/17257

Date: 1/1/1969

Abstract:
The Cascade Orchards Bridge is a continuous partially prestressed rigid fram concrete bridge constructed from cast-in-place concrete box girders and precast prestressed concrete girders field post-tensioned for structural continuity. A description of the structure, design criteria, and measurement results about the in-service performance of this bridge.