Post-Tensioned Waffle and Multispan Cantilever System with Y-Piers Composing the Hegenberger Overpass

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Post-Tensioned Waffle and Multispan Cantilever System with Y-Piers Composing the Hegenberger Overpass

Author(s): T.Y. Lin, Felix Kulka, and Y.C. Yang

Publication: Symposium Paper

Volume: 23

Issue:

Appears on pages(s): 495-506

Keywords: bridge piers; bridges (structures); concrete construction; long span; post-tensioning; precast concrete; prestressed concrete; reinforced concrete; skew bridges; structural analysis; structural design; waffle slabs

DOI: 10.14359/17250

Date: 1/1/1969

Abstract:
In the design of the Hegenberger Overpas (main span 290-ft) aesthetic and economic requirements justify the use of long spans to meet the curved alignment and the muliple crossings.