Title: Limit Design of Continuous Concrete Bridges Girders

Author(s): Kurt H. Gerstle and M.Z. Cohn

Publication: Symposium Paper

Volume: 23

Issue:

Appears on pages(s): 423-446

Keywords: bridges (structures); continuous beams; girders; limit design method (structural); moments; plastic analysis (structural); reinforced concrete; structural analysis; structural design

DOI: 10.14359/17247

Date: 1/1/1969

Abstract:
A limit design method for continuous reinforced concrete bridge girders is presented, which results in structures satisfying specified collapse and service conditions.