Fatigue Behavior of High Strength Deformed Bars in Reinforced Concrete Bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fatigue Behavior of High Strength Deformed Bars in Reinforced Concrete Bridges

Author(s): Masatane Kokubu, Hajime Okamura

Publication: Symposium Paper

Volume: 23

Issue:

Appears on pages(s): 301-316

Keywords: beams (structural), bending; bond (concrete to reinforcement); bridges (structures); cracking (fracturing); crack width and spacing; cyclic loads; deformations (reinforcing steel); deformed reinforcement; dynamic loads; fatigue (materials)

DOI: 10.14359/17241

Date: 1/1/1969

Abstract:
Results of bending fatigue and other tests of reinforced concrete beams using various high-strength deformed bars are presented.