Title: Can High-Strength Reinforcement Be Used in Highway Bridges?

Author(s): S.D. Lash

Publication: Symposium Paper

Volume: 23

Issue:

Appears on pages(s): 283-300

Keywords: beams (structural); bridges (structures); concrete durability; corrosion; cracking (fracturing); crack width and spacing; cyclic loads; deflection; fatigue (materials); flexural strength; high strength steels; highway bridges; loads (forces)

DOI: 10.14359/17240

Date: 1/1/1969

Abstract:
This paper summarizes the results of experiments carried out on beams reinforced with high-strength steel. . .It is concluded that high-strength reinforcement may be used in bridge construction with advantage.