Title: Torsional Analysis of Single Thin-Walled Trapezoidal Concrete Box-Girder Bridges

Author(s): David H.H. Tung

Publication: Symposium Paper

Volume: 23

Issue:

Appears on pages(s): 205-220

Keywords: bending; box beams; bridges (structures); deflection; deformation; diaphragms (concrete); girders; reinforced concrete; shear; stresses; structural analysis; torsion

DOI: 10.14359/17235

Date: 1/1/1969

Abstract:
A method is presented for the torsional analysis of single, thin-walled, trapezodial or rectangular concrete box-girder bridges which are symmetrical about the vertical axis of the cross-sections.