Title: Load Distribution in Concrete Box Girder Bridges

Author(s): A.C. Scordelis, R.E. Davis and K.S. Lo

Publication: Symposium Paper

Volume: 23

Issue:

Appears on pages(s): 117-136

Keywords: beams (structural); box beams; bridges (structures); computer programsl diaphragms (concrete); folded plates; girders; loads (forces); moments; reinforced concrete; specifications; stresses; structural analysis; structural design

DOI: 10.14359/17231

Date: 1/1/1969

Abstract:
Present design specifications and load distribution factors for reinforced concrete box girder bridges are critically reviewed.