A Five Year Study of the Dimensional Stability of Shrinkage-Compensating Lightweight Concrete Used in Post-Tensioned Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Five Year Study of the Dimensional Stability of Shrinkage-Compensating Lightweight Concrete Used in Post-Tensioned Slabs

Author(s): William P. Liljestrom, Milos Polivka

Publication: Symposium Paper

Volume: 38

Issue:

Appears on pages(s): 273-289

Keywords: concrete slabs; contraction; expansion; expansive cement type K; expansive cements; lightweight concretes; long-time study; post-tensioning; prestressed concrete; shrinkage; shrinkage-compensating concretes; tests

DOI: 10.14359/17208

Date: 1/1/1973

Abstract:
Commercial production of Type K expansive cement in the United States dates back to 1963, however it was not until three years later that a program of field measurements was undertaken in order to recorc the actual on-site concrete expansion and subsequent net length changes in two municipal structures using this shrinkage-compensating cement.