Study on the Optimum Restraint of Self-Stressed Concrete Pipe

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on the Optimum Restraint of Self-Stressed Concrete Pipe

Author(s): H. Iida, T. Monji

Publication: Symposium Paper

Volume: 38

Issue:

Appears on pages(s): 69-88

Keywords: concrete pipes; cracking (fracturing); expansive cement concretes; flexural strength; flexural tests; loads (forces); reinforced concrete pipes; restraints; self-stressing concretes; stresses

DOI: 10.14359/17199

Date: 1/1/1973

Abstract:
The objective of this study was to find the optimum restraining conditions for manufacturing self-stressed concrete pipe using expansive cement.