Method of Creep Analysis of Structural Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Method of Creep Analysis of Structural Members

Author(s): W. Dilger and A.M. Neville

Publication: Symposium Paper

Volume: 27

Issue:

Appears on pages(s): 349-372

Keywords: beams (supports); creep properties; deflection; deformation; prestressed concrete; reinforced concrete; shrinkage; strains; stress relaxation; stresses; structural analysis

DOI: 10.14359/17191

Date: 1/1/1971

Abstract:
The paper shows how data on creep and shrinkage of plain concrete can be used to calculate deformation of reinforced, including prestressed, concrete. It is assumed that the time dependent characteristics of the material (creep and shrinkage) are known and are available in a convenient form…