Title: Strengthening LaGuardia's Decks

Author(s): Kenneth Diao, Joseph Kelly, and Oscar Surds

Publication: Concrete International

Volume: 9

Issue: 10

Appears on pages(s): 39-42

Keywords: airports; repairs; runways; strengthening; taxiways; Construction

DOI:

Date: 10/1/1987

Abstract:
The runways at New York's LaGuardia Airport needed to be strengthened to support new heavier aircraft. A strengthening scheme was developed where grooves were cut in critical areas between existing reinforcing steel, and additional steel was installed. To