Construction of Precast Shells and Folded Plates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Construction of Precast Shells and Folded Plates

Author(s): Paul E. Mast

Publication: Symposium Paper

Volume: 28

Issue:

Appears on pages(s): 113-138

Keywords: barrel shells; concrete construction; connections; domes (structural forms); economics; elliptic parabolic shells; folded plates; hyperbolic parabolic shells; lift-slab construction; post-tensioning; precast concrete; prestressed concrete; shells

DOI: 10.14359/17152

Date: 1/1/1971

Abstract:
Virtually all common cast-in-place shell types have been built also as precast shells. Ample experience exists with such forms as precast long and short barrel shells, with elliptic and hyperbolic paraboloids, with spherical domes, with corrugated cylinders and, of course, with precast folded plates.