Title: Elastomeric Bearing Pad Connections in Precast Concrete Parking Structures

Author(s): James R. Libby

Publication: Concrete International

Volume: 9

Issue: 9

Appears on pages(s): 50-58

Keywords: bearings; connections; parking structures; precast concrete; plastics, polymers and resins; Design

DOI:

Date: 9/1/1987

Abstract:
Describes four instances of failure of elastomeric bearing pad connections in precast concrete parking structures. Areas needing research are enumerated and design and specification standards are called for.