Ferrocement Sunscreens on High-Rise Buildings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ferrocement Sunscreens on High-Rise Buildings

Author(s): M. A. Mansur, P. Paramasivam, and S. L. Lee

Publication: Concrete International

Volume: 9

Issue: 9

Appears on pages(s): 19-23

Keywords: buildings; connections; construction; ferrocement; sunscreens; structural design; Design

DOI:

Date: 9/1/1987

Abstract:
The first major field application of ferrocement in Singapore used precast ferrocement sunscreens to provide an economical and feasible solution to an unusual problem.