Behavior of Reinforced Concrete Frames with Reinforced Concrete Partial Infills

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Reinforced Concrete Frames with Reinforced Concrete Partial Infills

Author(s): Mehmet Emin Kara and Sinan Altin

Publication: Structural Journal

Volume: 103

Issue: 5

Appears on pages(s): 701-709

Keywords: frames; loads; reinforcement; seismic; strength; walls

DOI: 10.14359/16922

Date: 9/1/2006

Abstract:
The purpose of this research is to investigate the behavior of nonductile reinforced concrete (RC) frames strengthened by introducing partial infills under cyclic lateral loading. Seven one-bay, two-story, 1/3-scale test specimens were constructed and tested. The test frames had deficiencies commonly observed in residential RC buildings in Turkey. The aspect ratio of the infilled wall (lw/ hw , where lw = infill length and hw = infill height) and its placement configurations were the parameters of the experimental study. Test results revealed that partially infilled nonductile RC frames exhibited significantly higher ultimate strength and higher initial stiffness than the bare frame (frame with no infill). As the aspect ratio of the infilled wall increased, the lateral strength and the rigidity significantly increased. Strength and ductility inadequacies of the frame members influenced the lateral performance of the frame strengthened by partial infills. The most successful behavior was obtained from specimens with partially infilled walls connected to both the columns and beams of the frame.