Title: Thailand's Songkhla Bridges

Author(s): Chinawood Buranarom and Mogens Gissel

Publication: Concrete International

Volume: 9

Issue: 10

Appears on pages(s): 29-33

Keywords: bridges (structures); concrete construction; precast concrete; prestressed concrete; segmental construction; structural design; Design

DOI:

Date: 10/1/1987

Abstract:
The design and segmental construction of two precast, prestressed concrete box-girder bridges in southern Thailand are described. The south bridge is 940 m (3084 ft) long, with 22 40-m (131-ft) spans and two 30-m (98-ft) end spans. The north bridge is 170