Concrete Capacity Design (CCD) Approach for Fastening to Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Capacity Design (CCD) Approach for Fastening to Concrete

Author(s): Fuchs, W.; Eligehausen, R.; and Breen, J.

Publication: Commentary Reference

Volume: D

Issue: 9

Appears on pages(s): pp. 787–802.

Keywords:

DOI:

Date: 6/1/2008

Abstract:
ACI Structural Journal, V. 92, No. 1, Jan.-Feb. 1995, pp. 73–93. Also discussion, ACI Structural Journal, V. 92, No. 6, Nov.-Dec. 1995