234R-06: Guide for the Use of Silica Fume in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 234R-06: Guide for the Use of Silica Fume in Concrete

Author(s): ACI Committee 234

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 63

Keywords: curing; durability; high-range water-reducing admixture; high-strength concrete; placing; plastic-shrinkage cracking; silica fume; time of setting; water-reducing admixture; workability.

DOI:

Date: 4/13/2006

Abstract:
This report describes the physical and chemical properties of silica fume; how silica fume interacts with portland cement; the effects of silica fume on the properties of fresh and hardened concrete; recent typical applications of silica-fume concrete; how silica-fume concrete is proportioned, specified, and handled in the field; and areas where additional research is needed.