Title: Deformed Wire Fabric as Shear Reinforcement in Concrete Beams

Author(s): M. A. Mansur, C. K. Lee, and S. L. Lee

Publication: Structural Journal

Volume: 84

Issue: 5

Appears on pages(s): 392-399

Keywords: anchorage (structural); beams (supports); cracking (fracturing); crack width and spacing; deformed reinforcement; reinforced concrete; tests; shear properties; web reinforcement; welded wire fabric; Structural Research

DOI: 10.14359/1649

Date: 9/1/1987

Abstract:
The results of six full-size T-beams reinforced with bent-up deformed welded wire fabric (WWF) as stirrups are reported. The major parameters of the study were the amount of web steel and strength of the concrete. Test results indicate that the anchorages