Title: Bearing Design for the East Huntington Bridge

Author(s): David Goodyear

Publication: Symposium Paper

Volume: 94

Issue:

Appears on pages(s): 271-278

Keywords: bridge bearings; bridges (structures); precast concrete; cable-supported structures; composite construction (concrete and steel); specifications; structural design; Design

DOI: 10.14359/1644

Date: 9/1/1986

Abstract:
The bearing designs for a large, asymmetric concrete cable bridge are described. The special requirements for the support of a cable-stayed structure include vertical freedom in the cable-supported spans and longitudinal restraint for traffic and construction loads. The solution to these criteria is a specially designed horizontal bearing.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer