Trend of Highway Design

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Trend of Highway Design

Author(s): H. Eltinge Breed

Publication: Journal Proceedings

Volume: 19

Issue: 1

Appears on pages(s): 133-139

Keywords: none

DOI: 10.14359/16422

Date: 1/1/1923

Abstract:
The title contains an implication which is an admission-We are not satisfied with the roads we are building. Trend means change in a certain direction, and change involves two factors: inadequacy in present results; and new conditions requiring new adaptation of means to end.