Cement Posts

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cement Posts

Author(s): J.A. Mitchell, Goshen, Ind.

Publication: Journal Proceedings

Volume: 1

Issue: 1

Appears on pages(s): 39-41

Keywords: none

DOI: 10.14359/16420

Date: 1/1/1905

Abstract:
In presenting this paper upon the subject of cement posts I speak from practical experience, and will briefly give my views upon the subject. The knowledge I have of cement posts was obtained from an experience of over three years in the manufacture of them.