Coloring of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Coloring of Concrete

Author(s): J.P. Sherer, Milwaukee, Wis.

Publication: Journal Proceedings

Volume: 1

Issue: 1

Appears on pages(s): 11-15

Keywords: none

DOI: 10.14359/16414

Date: 1/1/1905

Abstract:
Representing the pioneer block manufacturing company of the Northwest, we have made many experiements in coloring artifical stone.