Hair Cracks, Crazing or Map Cracks on Concrete Surfaces

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Hair Cracks, Crazing or Map Cracks on Concrete Surfaces

Author(s): Albert Moyer

Publication: Journal Proceedings

Volume: 2

Issue: 1

Appears on pages(s): 208-213

Keywords: none

DOI: 10.14359/16406

Date: 1/1/1906

Abstract:
As an introduction to the subject to be discussed I do not think it would be amiss to say a word regarding what is popularly called artifical stone. Such introduction is more particularly appropriate for the reason that the strongest cement stone that can be made, and which more nearly resembles the natural product, unfortunately contains those qualities which, under the usual process of manufacturing cement stone, make the product more liable to those disfigurements which are best described as hair cracks or crazing. I would like to call your attention to the word "artifical stone." To my mind this word is objectionable; it does not describe and it is untrue.