Report of the Committee on Streets, Sidewalks and Floors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Report of the Committee on Streets, Sidewalks and Floors

Author(s): George L. Stanley, Chairman

Publication: Journal Proceedings

Volume: 4

Issue: 1

Appears on pages(s): 157-161

Keywords: none

DOI: 10.14359/16353

Date: 1/1/1908

Abstract:
In preparing specifications for sidewalks for adoption by our Association, it has been the aim of your committee to bring before you such specifications as, when followed, will result in good and serviceable sidewalks.