Effects of Two Non-Chloride Accelerating Agents on Setting Characteristics of Portland Cement Mortars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Two Non-Chloride Accelerating Agents on Setting Characteristics of Portland Cement Mortars

Author(s): Philip A. Smith

Publication: Symposium Paper

Volume: 102

Issue:

Appears on pages(s): 25-34

Keywords: accelerating agents; calcium chlorides; calcium nitrates; mortars (material); setting (hardening); sodium thiocyanates; Materials Research

DOI: 10.14359/1635

Date: 9/1/1987

Abstract:
Effects of two non-chloride accelerating agents -- sodium thiocyanate and calcium nitrate -- in time to achieve initial set of two brands of Type I cement were determined at 70 F (21 C) and 40 F (4 C). Results with these two non-chloride accelerators were compared with results with calcium chloride, the conventional accelerator. Tests show:Low or moderate dosages of the two non-chloride accelerators can reduce time to achieve initial set by l-2 hr.- Any one of the three accelerators may be more effective with one ce-ment than with another cement having similar setting characteristics without accelerators In general, all three of the accel-erators are more effective at 40 F than at 70 F.