Standard Specifications for Cement Hollow Building Blocks

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Standard Specifications for Cement Hollow Building Blocks

Author(s): ACI Committee on Specifications for Cement Hollow Building Blocks

Publication: Journal Proceedings

Volume: 5

Issue: 1

Appears on pages(s): 495-503

Keywords: none

DOI: 10.14359/16343

Date: 1/1/1909

Abstract:
Hollow cement blocks made in accordance with the folloiwng specifications, and meeting the requirements thereof, may be used in building construction, subject to the usual form of approval, required of other materials of construction, by the bureau of building inspection.