Costs of Reinforced Concrete Bridges Especially with Regard to Maintenance

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Costs of Reinforced Concrete Bridges Especially with Regard to Maintenance

Author(s): E. P. Goodrich, M. Am. Soc. C. E.

Publication: Journal Proceedings

Volume: 5

Issue: 1

Appears on pages(s): 219-240

Keywords: none

DOI: 10.14359/16326

Date: 1/1/1909

Abstract:
In an informal discussion on the subject of steel-concrete arches and other structures of similar composition, held at the Annual Convention of the American Society of Civil Engineers, June 26, 1906, two almost opposite opinions were expressed with regard to the relative costs of structural steel and of reinforced concrete for bridges.