Title: Decorative Concrete Stone

Author(s): Frederick A. Norris

Publication: Journal Proceedings

Volume: 5

Issue: 1

Appears on pages(s): 179-183

Keywords: none

DOI: 10.14359/16321

Date: 1/1/1909

Abstract:
It is now a generally accepted fact that properly made concrete possesses all qualities of the best natural quarried stone that would make it desirable as a building material with the exception of a pleasing appearance, which is often lacks.