Proposed Standard Specifications for Plain Concrete Drain Tile

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Standard Specifications for Plain Concrete Drain Tile

Author(s): ACI Committee on Specifications for Plain Concrete Drain Tile

Publication: Journal Proceedings

Volume: 6

Issue: 2

Appears on pages(s): 565-568

Keywords: none

DOI: 10.14359/16287

Date: 2/1/1910

Abstract:
The cement shall meet the requirements of the Standard Specifications for Portland Cement of the American Society for Testing Materials and adopted by this Association. (Standard No. 1.) This paper includes materials,proportions, mixing, forming, curing, dimensions, and finshed tile.