Title:
Report of the Committee on Building Laws and Insurance
Author(s):
ACI Committee on Building Laws and Insurance
Publication:
Journal Proceedings
Volume:
6
Issue:
2
Appears on pages(s):
343-348
Keywords:
none
DOI:
10.14359/16273
Date:
2/1/1910
Abstract:
The Committee on Building Laws and Insurance submits herewith revised Proposed Standard Building Regulations for the Use of Reinforced Concrete, for discussion and adoption.