Superplasticizers, Pozzolans, and Granulated Blast-Furnace Slags in Concrete: A Review

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Superplasticizers, Pozzolans, and Granulated Blast-Furnace Slags in Concrete: A Review

Author(s): V. M. Malhotra

Publication: Symposium Paper

Volume: 104

Issue:

Appears on pages(s): 63-88

Keywords: alkali-aggregate reactions; blast furnace slag; concretes; fly ash; plasticizers; pozzolans; reviews; roller compacted concrete; shotcrete; silica; Materials Research

DOI: 10.14359/1627

Date: 10/1/1987

Abstract:
Outlines the developments in superplasticizers, pozzolans, and granulated blast-furnace slags, and it describes how these materials have been used innovatively to improve the quality of concrete. Special reference is made to the development of high-streng