Concrete For Maritime Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete For Maritime Structures

Author(s): Chandler Davis

Publication: Journal Proceedings

Volume: 6

Issue: 2

Appears on pages(s): 120-157

Keywords: none

DOI: 10.14359/16262

Date: 2/1/1910

Abstract:
Intercourse between countries by water was developed almost as quickly as the travel by land, and as the size of ships increased the primitive method of beaching the vessel at high tide or hauling the ship out on the beach had to be adandoned and artifical landing places built.