Title: Proposed Standard Specifications for Architectural Concrete Stone

Author(s): ACI Committee on Specifications for Architectural Concrete Stone

Publication: Journal Proceedings

Volume: 7

Issue: 12

Appears on pages(s): 766-769

Keywords: none

DOI: 10.14359/16248

Date: 12/1/1911

Abstract:
The specification is intended to cover the general requirements for quality of material and products for the manufacture of Concrete Stone, commonly termed Artificial Stone, by the two generally accepted methods known as the WET and DRY process.