Title: Ground Granulated Blast-Furnace Slag as a Cementitious Constituent in Concrete

Author(s): ACI Committee 226

Publication: Materials Journal

Volume: 84

Issue: 4

Appears on pages(s): 327-342

Keywords: blast-furnace slag; concretes; granular materials; iron; mix proportioning; mortars (material); pelleting; portland cements; specifications; Materials Research

DOI: 10.14359/1623

Date: 7/1/1987

Abstract:
The use of iron blast-furnace slag as a constituent of concrete, either as an aggregate or as a cementing material, or both, is well known. The use of ground granulated blast-furnace (GGBF) slag in the production of blended cements began in 1905 in the Un