Resolutions Relative to the Uniform Designation of the Binding Materials Used in The Preparation of Concrete and Other Resolutions Governing the Uniform Transportation and Examination of Cements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Resolutions Relative to the Uniform Designation of the Binding Materials Used in The Preparation of Concrete and Other Resolutions Governing the Uniform Transportation and Examination of Cements

Author(s): Society of Hungarian Enigneers and Architects

Publication: Journal Proceedings

Volume: 7

Issue: 12

Appears on pages(s): 468-502

Keywords: none

DOI: 10.14359/16228

Date: 12/1/1911

Abstract:
Lime is the product obtained from the calcination of limestones. When moistened with water it evolves great heat with extension of volume, resolving into fine powder. Upon the addition of more water it assumes with similar phenomena a paste-like consistency. Lime is placed on the market either in lumps or, when hydrated, in powder form and also as slaked lime in pastry form, depending on local requirements.