Problems Encountered in Concstructing the Aziscohos Storage Dam

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Problems Encountered in Concstructing the Aziscohos Storage Dam

Author(s): Seth A. Moulton

Publication: Journal Proceedings

Volume: 7

Issue: 12

Appears on pages(s): 274-310

Keywords: none

DOI: 10.14359/16217

Date: 12/1/1911

Abstract:
The new reservoir, which will be created by the construction of the Aziscohos Dam, will be a unit in the comprehensive system of water storage which has been developed at the head waters of the Androscoggin River. The scope of this paper will not permit a detailed description of the entire storage project; but it is necessary, for a thorough understanding of the subject in hand, that a brief history be given of the original enterprise and its relation to the work now in progress, which this paper purports to describe. For convenience of presentation it will be subdivided into six general headings which will be discussed in the order named, as follows: 1. History 2. Organization 3. Transportation 4. Design 5. Logging 6. Construction