Cement Paving as Construction at Mason City, Iowa

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cement Paving as Construction at Mason City, Iowa

Author(s): F.P. Wilson

Publication: Journal Proceedings

Volume: 8

Issue: 3

Appears on pages(s): 689-693

Keywords: none

DOI: 10.14359/16190

Date: 3/1/1912

Abstract:
For the past five or six years the writer has made a broad study of cement paving and has visited a large number of cities in the Northern States where this class of pavement has been laid and has watched the methods of construction in detail for this class of pavements.