Title: Standard Specifications for Concrete Curb and Concrete Curb and Gutter

Author(s): ACI Committee on Specifications for Concrete Curb and Concrete Curb and Gutter

Publication: Journal Proceedings

Volume: 8

Issue: 3

Appears on pages(s): 658-664

Keywords: none

DOI: 10.14359/16186

Date: 3/1/1912

Abstract:
The cement shall meet the requirements of the Standard Specifications for Portland Cement of the American Society for Testing Materials and adopted by this Association. (Standard No. 1.) This paper includes materials,sub-grade, sub-base, forms, construction, measuring and mixing, two-course curb and gutter, wearing course, one-course curb and gutter, and protection.