Review of the Present Status of Iron Ore Cement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Review of the Present Status of Iron Ore Cement

Author(s): P.H. Bates

Publication: Journal Proceedings

Volume: 8

Issue: 3

Appears on pages(s): 566-577

Keywords: none

DOI: 10.14359/16178

Date: 3/1/1912

Abstract:
It is generally understood that there are three essential constitutents in Portland cement, namely: lime, alumina, and silica. It has been shown experimentally that the lime can be entirely replaced by strontium or barium, the alumina in part by iron or chromium oxide, and hydraulic materials of considerable value be obtained; but none of these have been suggested as being of commerical value with the exception of iron oxide.