Report of Committee on Treatment of Concrete Surfaces

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Report of Committee on Treatment of Concrete Surfaces

Author(s): ACI Committee on Treatment of Concrete Surfaces

Publication: Journal Proceedings

Volume: 8

Issue: 3

Appears on pages(s): 539-546

Keywords: none

DOI: 10.14359/16176

Date: 3/1/1912

Abstract:
The Committee has this year devoted itself to perfecting specifications for stucco and to methods of testing compounds for dampproofing of surfaces. Every member of the Association who was known to have knowledge on these subjects was written to, something over four hundred persons being addressed. There was no real criticism from anyone, and we therefore feel justified in recommending this specification for adoption this year.