Title: Comparative Tests of the Strength of Concrete in the Laboratory and in the Field

Author(s): Rudolph J. Wig

Publication: Journal Proceedings

Volume: 8

Issue: 3

Appears on pages(s): 522-525

Keywords: none

DOI: 10.14359/16174

Date: 3/1/1912

Abstract:
It is common practice at the present time to define a desired strength of concrete by stating that it shall be made of good quality materials in certain given proportions.