Report of Committee on Specifications and Methods of Tests for Concrete Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Report of Committee on Specifications and Methods of Tests for Concrete Materials

Author(s): ACI Committee on Specifications and Methods of Tests for Concrete Materials

Publication: Journal Proceedings

Volume: 8

Issue: 3

Appears on pages(s): 473-485

Keywords: none

DOI: 10.14359/16171

Date: 3/1/1912

Abstract:
In this first report of the Committee no definite recommendations are presented for specific tests or methods are presented for specific tests or methods of making tests of aggregate, except that the Committee recommends for a practical test of sand a determination of the strength of mortar made with it. The report, therefore, is in the nature of a tenative discussion of various tests and of methods that have been used in different laboratories. This progress report should be followed during the coming year by further investigations leading to more definite recommendations.