Unit Costs of Reinforced Concrete For Industrial Buildings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Unit Costs of Reinforced Concrete For Industrial Buildings

Author(s): Chester S. Allen

Publication: Journal Proceedings

Volume: 8

Issue: 3

Appears on pages(s): 400-405

Keywords: none

DOI: 10.14359/16165

Date: 3/1/1912

Abstract:
Unit costs are harmless when used with judgment and prudence, but likley to bring remorse and anguish when employed prmiscuously. Rare and talented indeed is the man who possess the experience, judgement and intuitive sense to know when, where and how to properly modify any tables or statements of unit costs to meet the peculiar conditions of each individual case.