Investigation of Complete Stress-Deformation Curves for Concrete in Tension

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Investigation of Complete Stress-Deformation Curves for Concrete in Tension

Author(s): Guo Zhen-Hai and Zhang Xiu-Qin

Publication: Materials Journal

Volume: 84

Issue: 4

Appears on pages(s): 278-285

Keywords: concretes; cracking (fracturing); deformation; stiffness; stress-strain relationships; tensile strength; tension; tension tests; Materials Research

DOI: 10.14359/1616

Date: 7/1/1987

Abstract:
Complete stress-deformation curves for concrete were measured from direct tension tests under both monotonic and cyclic loading. The initiation and propagation of cracking on the surface of specimens were observed during the tests. Tensile strength and co